• ulu_fanua_01

INCOLOY® u'amea 800H/800HT UNS N08810/UNS N08811

Fa'amatalaga Puupuu:

INCOLOY alloys 800H ma 800HT e sili atu le maualuga o le fetolofi ma le malepelepe malosi nai lo le INCOLOY alloy 800. O u'amea e tolu e toetoe lava a tutusa le fa'aogaina o vaila'au.


Fa'amatalaga Oloa

Faailoga o oloa

Fa'asu'esu'ega o vaila'au

Alloy elemene C Si Mn S Cu Ni Cr Al Ti Fe Al+Ti

Incoloy800H/HT

Min 0.05         30.0 19.0 0.15 0.15 39.0 0.30
Max 0.10 1.0 1.5 0.05 0.75 35.0 23.0 0.60 0.60   1.20
Fa'amatalaga Incoloy 800HT:C:0.06~0.10,Al+Ti:0.85~1.20.

Meatotino Fa'ainisinia

Aolly Tulaga

Malosi fa'asa

Rm MpaMin

Tuuina atu le malosi

RP 0. 2 Mpa Min

Fa'aumiumi

A 5%Min

fa'atosina

448

172

30

Meatotino Faaletino

Malosig/cm3

Lisi Lisi

7.94

1357~1385

Tulaga

O'oto'o, Pa, Uaea ma Fa'atauga- ASTM B 408 & ASME SB 408 (Rod & Bar), ASTM B 564 & ASME SB 564 (Forgings)

Papatusi, Pepa ma Fa'ailoga -ASTM A240/A 480 & ASME SA 240/SA 480(Ipu, Pepa, ma le Fa'asolo), ASTM B 409/B906 & ASME SB 409/SB 906 (Pautusi, Pepa, ma le Fa'asolo)

Paipa & Paipa- ASTM B 407/B829 & ASME SB 407/SB 829 (Pipa Seamless & Pipa), ASTM B 514/B 775 & ASME SB 514/SB 775 (Pipa Uila), ASTM B 515/B 751 & ASME SB 515/ (Tupa Uila)

Isi Fomu Oloa -ASTM B 366/ASME SB 366 (Fa'aoga)

Uiga o Incoloy 800H/Incoloy 800HT

Falegaosi oloa Incoloy maualuga

● Malosi maualuga o le vevela

● Malosi o le fetolofi maualuga

● Tetee i oxidation ma carburization i siosiomaga vevela maualuga

● Tete'e lelei corrosion i le tele o siosiomaga acidic

● Lelei e tetee atu i le tele o ea e maua i le sulfur


  • Muamua:
  • Sosoo ai:

  • Tusi lau savali iinei ma lafo mai ia i matou

    oloa fa'atatau

    • INCOlOY® u'amea 825 UNS N08825/W.Nr. 2.4858

      INCOlOY® u'amea 825 UNS N08825/W.Nr. 2.4858

      INCOLOY alloy 825 (UNS N08825) o se nickel-iron-chromium alloy faatasi ai ma faʻaopoopoga o le molybdenum, kopa, ma le titanium .Ua mamanuina e tuʻuina atu ai le tetee faʻapitoa i le tele o siosiomaga pala. Ole mea ole nickel e lava mo le tetee atu ile chloride-ion stress-corrosion ta'e. O le nickel faʻatasi ma le molybdenum ma le kopa, e tuʻuina atu ai foʻi le teteʻe mataʻina i le faʻaitiitia o siosiomaga e pei o loʻo i ai sulfuric ma phosphoric acids. O le molybdenum e fesoasoani foi i le tetee atu i le pala ma le gaogao. O le chromium o lo'o i totonu o le u'amea e tu'uina atu ai le tete'e atu i le tele o mea fa'ama'i e pei ole nitric acid, nitrates ma le masima fa'ama'i. O le fa'aopoopoga o le titanium e aoga, fa'atasi ai ma se togafiti vevela talafeagai, e fa'amautu ai le u'amea e fa'asaga i le fa'alogoina i le fa'aleagaina o le va'aiga.

    • INCOLOY® fa'afefiloi A286

      INCOLOY® fa'afefiloi A286

      INCOLOY alloy A-286 o se uʻamea-nickel-chromium uʻamea faʻatasi ma faʻaopoopoga o le molybdenum ma le titanium. E fa'ama'a'a tausaga mo mea fa'ainisinia maualuga. O le u'amea e fa'atumauina lelei le malosi ma fa'ama'i fa'ama'i i le vevela e o'o atu ile 1300°F (700°C). O le u'amea e austenitic i tulaga metallurgical uma. O le malosi maualuga ma uiga sili ona lelei o le gaosiga o le INCOLOY alloy A-286 e faʻaogaina ai le faʻaoga mo vaega eseese o vaalele ma kesi kesi fale gaosi oloa. E fa'aogaina fo'i mo fa'aoga fa'amau i totonu o masini ta'avale ma vaega fa'atele e fa'atatau i le maualuga o le vevela ma le fa'alavelave ma i totonu o le suau'u ma kesi i fafo.

    • INCOLOY® u'amea 254Mo/UNS S31254

      INCOLOY® u'amea 254Mo/UNS S31254

      254 SMO pa'u u'amea u'amea, lea e ta'ua o le UNS S31254, na muamua fa'atupuina mo le fa'aoga i le sami ma isi si'osi'omaga fa'amalosi e maua ai le chloride. O lenei vasega ua manatu o se u'amea austenitic pito sili ona maualuga; UNS S31254 e masani ona taʻua o le "6% Moly" grade ona o le molybdenum content; o le 6% Moly aiga o loʻo i ai le malosi e tatalia ai le maualuga o le vevela ma faʻamautu le malosi i lalo o tulaga faʻafefe.

    • INCOLOY® u'amea 800 UNS N08800

      INCOLOY® u'amea 800 UNS N08800

      INCOLOY alloy 800 (UNS N08800) o se mea faʻaaogaina lautele mo le fausiaina o meafaigaluega e manaʻomia ai le faʻafefeteina, vevela vevela, malosi, ma le mautu mo le tautua e oʻo atu i le 1500 ° F (816 ° C). Alloy 800 o lo'o ofoina atu le fa'atosina lautele i le tele o fa'asalalauga vai ma, ona o lona anotusi o le nickel, e tete'e atu ai i le ta'e a'e. I le maualuga o le vevela e ofoina atu ai le tetee atu i le faʻamaʻiina, carburization, ma le sulfidation faʻatasi ai ma le gau ma le malosi fetolofi. Mo talosaga e mana'omia ai le malosi e tetee atu ai i le malepelepe ma le fetolofi, aemaise i le vevela i luga atu o le 1500°F (816°C).

    • INCOLOY® u'amea 925 UNS N09925

      INCOLOY® u'amea 925 UNS N09925

      INCOLOY alloy 925 (UNS N09925) o se nickel-u'amea-chromium fa'amaaa tausaga ma fa'aopoopoga o le molybdenum, kopa, titanium ma le alumini. Ua mamanuina e tuʻuina atu ai se tuʻufaʻatasiga o le malosi maualuga ma sili atu le faʻafefeteina. O mea o lo'o i totonu o le nickel ua lava mo le puipuiga mai le chloride-ion stress corrosion ta'e. O le nickel, faʻatasi ma le molybdenum ma le kopa, e tuʻuina atu ai foʻi le teteʻe mataʻina i le faʻaitiitia o vailaʻau. O le molybdenum e fesoasoani i le tetee atu i le pala ma le gaogao. Ole mea ole chromium alloy e maua ai le tetee ile siosiomaga fa'ama'i. O faʻaopoopoga o le titanium ma le alumini e mafua ai le faʻamalosia o le gaioiga i le taimi o togafitiga vevela.